Product catalog summary
Overview of Multi Cell Differential Scanning Calorimetry (MCDSC):
The MCDSC is a versatile microcalorimeter designed for continuous temperature-scanning, step-scanning, or isothermal measurements. It can analyze three samples and one reference simultaneously, with a sample capacity of one milliliter and microwatt sensitivity. This allows for the identification of phase transitions, metabolic activity, and thermal events in complex reactions. The device offers superior baseline stability and rapid temperature changes, with reusable and high-pressure ampoules for diverse experimental designs.
Specifications:
  • Sample Cells: 3
  • Reference Cells: 1
  • Temperature Range: -40 to 150 °C
  • Detection Limit: 0.2 μW
  • Cell Volume: 1 ml
  • Sample Volume: up to 1 ml
  • Short Term Noise Level: 0.2 μW
  • Baseline Repeatability: 2 μW
  • Scan Rate: 0 to 2 ºC/minute
  • Response Time: 90 seconds or 9 minutes for 99% response
  • Heat Measurement Method: Heat flux
Technology and Features:
The MCDSC uses Peltier technology for temperature control and heat detection, allowing precise isothermal operation and reproducible scan rates. It features four removable cells and Hastelloy ampoules with O-rings for hermetic sealing, suitable for high-pressure applications. The ampoules are resistant to corrosion and inert to biological materials.
Ampoules:
  • Standard Ampoules: Hastelloy®, 1.0 ml volume
  • High Pressure Ampoules: Hastelloy®, 0.5 ml volume, max pressure 6000 psi
  • Probe Accessible Ampoules: For pressure measurements and connections to analytical instruments
  • Batch Reaction Ampoules: For studying reactions between solids, liquids, and vapors
Applications:
  • Drug-Excipient Compatibility: Rapid determination of reaction rates and temperature dependence in drug formulations.
  • Biofuel Production: Analysis of reaction kinetics in biofuel production processes.
  • Shelf-Life Prediction: Step-scanning method for determining activation energies and reaction mechanisms.
  • Polymorph & Amorphous Crystallization: Measurement of heat and kinetics in reactions involving volatile substances.
  • Metabolic Rate Analysis: Continuous temperature scans for optimizing conditions in biological studies.
  • Food Processing: Determination of reaction rates for optimizing storage and manufacturing conditions.
  • Phase Transitions in Foods: Analysis of phase transitions affecting food quality.
References:
The document includes a comprehensive list of references related to microcalorimetry applications and studies, highlighting the instrument's versatility in various scientific fields.
See more

Catalog excerpts

MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-1

2012 Micro Cal cover_Layout 1 7/10/12 11:29 AM Page 2

 Open the catalog to page 1
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-2

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:18 AM Page 48

 Open the catalog to page 2
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-3

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:18 AM Page 49 MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY The MCDSC is a versatile, multipurpose microcalorimeter that provides continuous temperature-scanning, step-scanning or isothermal measurements on three samples and one reference simultaneously. The one milliliter sample capacity ampoules and microwatt sensitivity ensures maximum flexibility for identifying phase transitions in chemicals and biologicals, metabolic activity in cellular organisms and thermal events occurring in complex reactions of liquids and/or solids during admixing. The...

 Open the catalog to page 3
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-4

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:18 AM Page 50

 Open the catalog to page 4
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-5

Short Term Noise Level 0.2 uW Scan Rate 0 (isothermal) to 2 °C/minute Response Time 90 second time constant or 9 minutes for 99% response Heat Measurement Method Heat flux

 Open the catalog to page 5
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-6

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:18 AM Page 52 No other DSC on the market offers more flexibility for studying thermal stability of almost any sample as a function of temperature or time. The calorimeter exploits ultra-sensitive Peltier technology for both temperature control and as sensors to detect heat effects. Peltier cascades allow precise temperature control for isothermal operation and reproducible scan rates up to 2 ºC per minute. The Peltier sensors give true microwatt detection independent of scan rate. Equipped with four removable cells, this is truly a workhorse instrument....

 Open the catalog to page 6
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-7

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:18 AM Page 53 Standard Ampoules High Pressure Ampoules Probe Accessible Ampoules Batch Reaction Ampoules Hastelloy®, 1.0 ml volume, 11mm diameter, 5mm depth Hastelloy®, 0.5ml volume, Kalrez® O-rings, max pressure 6000psi Standard Ampoule with special connections for pressure measurements, and connecting to spectrophotometers, mass specs, and gas chromatographs. Special Hastelloy® cells with two separate, sealed compartments for studying the reaction (and heat of reaction) between solids, liquids, and vapors.

 Open the catalog to page 7
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-8

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:18 AM Page 54 MC DSC Applications Drug-Excipient Compatibility 10 Reaction Heat Rate (µW/mg) Because of the large sample capacity and multiple cell design, the MC DSC can be used to rapidly determine the temperature dependence of rates of drug-excipient reactions. This figure shows the results from a continuous temperature scan of 155mg of a 1:1 mixture of aspirin and magnesium stearate. The rate of the endothermic reaction indicating incompatibility becomes measurable at about 50 ºC. Because of the wide-mouth (11mm) and depth (5mm) of the ampoules,...

 Open the catalog to page 8
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-9

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:19 AM Page 55 Shelf-Life Prediction by Step-Scanning 2500 Reaction Heat Rate (µW/g) In the step-scan method, the calorimeter temperature is rapidly scanned to a programmed temperature and then held isothermal for sufficient time (30-45 min) to allow for equilibration to accurately measure the steady-state heat rate, then stepped to the next temperature for another measurement of the isothermal heat rate. Step-scan measurements are particularly useful for accurate determination of activation energies and temperatures at which reaction mechanisms change....

 Open the catalog to page 9
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-10

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:19 AM Page 56 MC DSC Applications Temperature Dependence of Metabolic Rate In many organisms, metabolic heat rate is equivalent to the oxygen uptake rate, but heat rate is much easier to measure in cell cultures, tissues, and small organisms. Data on respiration rate as a continuous function of temperature is necessary to optimize conditions for cell cultures, for prediction of the effects of climate change on organisms and ecosystems, for selection of cultivars of crop plants for optimum productivity, and for prediction of the invasive potential...

 Open the catalog to page 10
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-11

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:19 AM Page 57 Determination of the temperature dependence of reaction rates is necessary for establishing proper storage, manufacturing, and compounding conditions for foods, drugs, cleaners, and industrial chemicals and products. The rates of reactions in diverse materials can be rapidly determined as a continuous function of temperature with the MC DSC. Continuous scanning is particularly useful for rapidly establishing the optimal temperatures for more definitive, but much slower, determinations of the identity of reactions and of rate laws by...

 Open the catalog to page 11
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-12

Micro Brochure 2012 WHITE_Layout 1 7/10/12 11:19 AM Page 58 REFERENCES Garbett, N., DeLeeuw, L. and J.B. Chaires. MCAPN-2010-04. High-throughput DSC: A Comparison of the TA Instruments Nano DSC Autosampler System™ with the GE Healthcare VP-Capillary DSC™ (2010) Demarse, N. and L.D. Hansen. MCAPN-2010-01. Analysis of Binding Organic Compounds to Nanoparticles by Isothermal Titration Calorimetry (ITC). (2010) Quinn, C.F. MCAPN-2010-02. Analyzing ITC Data for the Enthalpy of Binding Metal Ions to Ligands. (2010) Quinn, C.F. and L.D. Hansen. MCAPN-2010-03. Pressure Perturbation Calorimetry: Data...

 Open the catalog to page 12
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-13

2012 Micro Cal cover_Layout 1 7/10/12 11:29 AM Page 4

 Open the catalog to page 13
MULTI CELL DIFFERENTIAL SCANNING CALORIMETRY-14

2012 Micro Cal cover_Layout 1 7/10/12 11:28 AM Page 1 © 2012 TA Instruments. All rights reserved.

 Open the catalog to page 14
*Prices are pre-tax. They exclude delivery charges and customs duties and do not include additional charges for installation or activation options. Prices are indicative only and may vary by country, with changes to the cost of raw materials and exchange rates.
About DirectIndustry
DirectIndustry is a marketplace that offers B2B players a complete experience, from product sourcing to purchase. DirectIndustry is an entity of VirtualExpo Group.