Tritone Industrial Additive Manufacturing Material datasheet Composition - According to ASTM A276-06 — — ASSINTERED. HEAT TREATED Typical Mechanical Properties Standard ge'sintered heat treated as sintered HI300 Ultimate Tensile Strength,MPa Relative density, % * Properties of as sintered material are affected by the cooling rate of the sintering process. * AISI 4340 alloy steel is heat treated at 840°C (1544°F) followed by quenching under Nitrogen. All tests were performed in independent professional laboratories to verify ‘as-sintered’ and composition data. Microstructure images were etched and photographed at an external facility. Subject to change without

 Open the catalog to page 1

All Tritone Technologies catalogs and technical brochures

*Prices are pre-tax. They exclude delivery charges and customs duties and do not include additional charges for installation or activation options. Prices are indicative only and may vary by country, with changes to the cost of raw materials and exchange rates.