Removing the Anodic Oxidation of Aluminum Marking Requirement: Remove the Anodic Oxidation of Aluminum with high speed; without introduce curvature on cosmetic surface of PAD. Marking Matrix F-Lens: F254MM Power: <20W Pulse width: 8ns Frequency: 100kHz Marking Speed: 5000mm/s After laser removing Surface curvature after laser treatment Laser Anodic oxidation