Catalog excerpts
ARGWELD® BACKING TAPE One way to improve quality and productivity in sheet metalwork large diameter pipework and vessels. Use Argweld® Backing Tape •Eliminate 2 sided welding• •No more back purging• •Flat, coke free welds• •Reduction of manufacturing costs• •No post weld grinding necessary• See overleaf for step by step approach
Open the catalog to page 1Step 1 - Apply Simply stick the tape onto the clean weld joint area. Step 2 - Weld Weld onto tape casting molten weld pool onto tape to obtain flat, coke free, pore free weld, which needs no grinding. Step 3 - Remove Remove tape to see a flat well formed bead with light cleaning as required. Huntingdon Fusion Techniques Limited, Stukeley Meadow, Burry Port, Carms SA16 0BU United Kingdom Telephone: +44 (0) 1554 836 836 Facsimile: +44 (0) 1554 836 837 Email: hft@huntingdonfusion.com http://www.huntingdonfusion.com Copyright © 2000-2002 All rights reserved. This publication may not be...
Open the catalog to page 2All Huntingdon Fusion Techniques catalogs and technical brochures
-
ARGWELD® FLEXIBLE ENCLOSURE
1 Pages
-
FLEXIBLE WELDING ENCLOSURES
2 Pages
-
processing and processors
4 Pages
-
WELD BACKING TAPE 2010
2 Pages
-
WELD BACKING TAPE 2009
2 Pages
-
WELD BACKING TAPE 2011
2 Pages
-
purge eye 600
2 Pages
-
purge eye 500
2 Pages
-
purge eye 300
2 Pages
-
purge eye 300 nano
2 Pages
-
purge elite
4 Pages
-
Product Overview
2 Pages
-
Weld Purge Monitor MKV
2 Pages