Cordenka® rayon is a man-made cellulose yarn used in technical applications, consisting of multiple continuous filaments. It is available in various forms, including woven fabrics and chopped fibers.
FeaturesIncludes details on linear density, number of filaments, breaking force, tensile strength, elongation at break, and tensile modulus for different grades of Cordenka® yarn.
PackagingProducts are packaged in cylindrical bobbins with specific pallet dimensions and weights.
DisclaimerCordenka provides technical data believed to be accurate as of the document's issue date but reserves the right to update it. No warranty is made regarding the suitability of products for specific purposes.
Contact InformationFor further information, contact Cordenka via phone, email, or their website.
* -premium rayon reinforcement General Description Storage, Handling and Processing Cordenka® rayon is a man-made cellulose yarn for technical applications. It consists of multiple continuous filaments. The number of filaments determines the linear density of the yarn, i.e. its thickness (1 dtex = 10-4 g m-1). Usually the yarn has almost no twist (approx. 2-3 t/m) so that the single filaments are aligned in parallel. We can also provide twisted yarns (100 t/m). Furthermore we offer Cordenka® rayon in form of woven fabrics and chopped fibers. • Specified constant properties • Improvement of composite material's ♦ Impact resistance, also at low temperatures • Reinforcement and light weight construction for: ♦ Completely biobased and biodegradable composites ♦ Passenger car tyres, mechanical rubber goods • Vehicle parts, shields, housing for machinery • Acoustic devices, sports equipment • Cordenka® rayon is composed of cellulose. It is both • Storage: Protect CORDENKA® products against heat, cold, moisture, direct solar radiation and extreme climatic fluctuations. • Cutting and dosing: For Cutting and dosing of Cordenka® Rayon we recommend the use of special equipment. If you need assistance for selecting appropriate machinery, please contact us. • Processing: If your process is sensitive to moisture, we recommend drying of Cordenka® rayon for two hours at 105 °C. Alternatively, inline drying at higher temperatures (less than a minute) can be applied. During processing, the temperature should be kept below 200 °C and the exposure time at this temperature should not exceed 20 minutes. • For the compounding of thermoplastic composites it might be useful to add coupling agents. Excellent results in polypropylene can be achieved with MAHPP. Superior recycling suitability: During processing, Cordenka® rayon maintains an excellent level of fiber lengths, resulting in a consistently high level of mechanical properties in
Open the catalog to page 1-premium rayon reinforcement Further Information phone: +49 60 22 81 3264 mail: [email protected] web: www.cordenka.com ©2021 Cordenka GmbH & Co. KG - All rights reserved. Cordenka GmbH & Co. KG (“Cordenka”) believes that the technical data and other information provided herein was materially accurate as of the date this document was issued. Cordenka reserves the right to update, revise or modify such technical data and information at any time. Any performance values provided are considered representative but do not and should not constitute a substitute for your own testing of the suitability...
Open the catalog to page 21 Page