| | | O-Ring | | |
| | | |
| | | |
| | | B.1.2 Application parameters of elastomers Elastomers as all other organic chemicals have limited use. External influences such as various media, oxygen or ozone as well as pressure and temperature will affect the material properties and therefore their sealing capability. | | |
| | | Elastomers will amongst others swell, shrink or harden and develop cracks or even tears. The following information illustrates the different application parameters. | | |
| | | |
| | | Elastomer heat resistance / swelling in oil | | |
| | | |
| | | Figure 3 Change of volume in IRM-Oil 903 (old ASTM-Oil No 3) | | |
| | | |
| | | W//A | | |
| | | Latest information available at www.tss.trelleborg.com Edition June 2008 | | |