Composite Welder FS - 15203 Composite Welder FS

Description: A 2-component 10:1 flexible methacrylate adhesive with fast fixturing and cure times. Intended Use: Bonds steel furniture, speaker magnets, and dissimilar substrates. Bonds FRP/GRP/SMC, gel coat, honeycomb painted and plated metals (with primer), phenolics, polycarbonate, PVC polyesters, urethanes and vinyl esters along with ceramics. Product features:Excellent environmental resistanceExcellent impact, peel, and shear resistanceSuperb salt spray durability, including aluminumTypical PhysicalProperties: Limitations: Surface Preparation: Technical data should be considered representative or typical only and should not be used for specification purposes. Cured 7 days @ 75° F TESTS CONDUCTED ColorViscosityWeightMixed ViscosityMix Ratio by VolumeMix Ratio by WeightMixed Density FlashpointWorking TimeFixture Time Functional CureFull CureService Temperature T-peelImpact Resistance Tensile ElongationShore HardnessGap-Fill % Solids by VolumeAdhesive Tensile Lap Shear [galvanized]Adhesive Tensile Lap Shear[AL] Adhesive Tensile Lap Shear[GBS]Adhesive Tensile Lap Shear[SS]Specfic VolumeBlue/GreenAdhesive: 120,000 cps: Activator: 60,000 cps Adhesive:8.0/lbs./gal.; Activator: 8.95lbs./gal.120,000 cps10:189:108.09 lbs/gal / 0.97gm/cc51°F4-8 min. @ 75°F 10-15 min. @ 75°F3/4 - 1 hrs.24 hours -40°F to 250°F 60-65 pli22 ft.lb./in.[2] 100-125%74 Shore D.375 in. 100 %2,000 psi [with MP 90]2,525 psi [with MP 90] 2,250 psi2,800 psi [with MP 90]28.55 in[3]/lb. Uncured Clean surface by solvent-wiping any deposits of heavy grease, oil, dirt, or other contaminants. Surface can also be cleaned with industrial cleaning equipment such as vapor phase degreasers or hot aqueous baths. If working with metal, abrade or roughen the surface to significantly increase the microscopic bond area and optimize the bond strength. Mixing Instructions: ---- Proper homogenous mixing of resin and hardener is essential for the curing and development of stated strengths. ----25 ML DEV-TUBE1. Squeeze material into a small container the size of an ashtray. 2. Using mixing stick included on Dev-tube handle, vigorously mix components for one (1) minute.3. Immediately apply to substrate.35ML/50 ML/250 ML/380 ML/400 ML CARTRIDGES1. Attach cartridge to Mark V™ [50ml], 380ml, 250ml [15:1 caulk gun], or 400ml dispensing systems [manual or pneumatic]. 2. Open tip.3. Burp cartridge by squeezing out some material until both sides are uniform (ensures no air bubbles are present during Adhesive Tensile Shear ASTM D 1002Cured Hardness Shore D ASTM D 2240T-Peel Strength ASTM D 1876 Impact Resistance ASTM D 950 ITW Devcon, 30 Endicott Street, Danvers, MA 01923 Tel:(978) 777-1100 Fax:(978) 774-0516 www.devcon.com

pageCatalog pdf di En 2012-02-07-13